The ceramic brittleness of the pressed and sintered yttria zirconia-mullite-magnesia system
Hakim B.L.a, Soepriyanto S.a, Korda A.A.a, Sunendar B.a
a Department of Metallurgical Engineering, Faculty of Mining and Petroleum, Bandung Institute of Technology, Bandung, 40132, Indonesia
[vc_row][vc_column][vc_row_inner][vc_column_inner][vc_separator css=”.vc_custom_1624529070653{padding-top: 30px !important;padding-bottom: 30px !important;}”][/vc_column_inner][/vc_row_inner][vc_row_inner layout=”boxed”][vc_column_inner width=”3/4″ css=”.vc_custom_1624695412187{border-right-width: 1px !important;border-right-color: #dddddd !important;border-right-style: solid !important;border-radius: 1px !important;}”][vc_empty_space][megatron_heading title=”Abstract” size=”size-sm” text_align=”text-left”][vc_column_text]© 2015 AIP Publishing LLC.The brittleness behaviour of the pressed and sintered Yttria Zirconia-Mullite-Magnesia system has been studied. Specifically, the brittleness index represents a correlation of material properties for predicting mechanical properties such as for the characterization of machinability, wear or erosion resistance. The brittleness index as well as fracture toughness were obtained from indentation testing of the Vickers hardness. In this study, the fracture toughness considered the crack extension mechanism to accommodate Palmqvist crack criteria for the measured data. The additional of Mullite at amount of 15% into 3Y-TZP system significantly reduces the brittleness index while compared to pure Mullite system up to 69%. In the other hand, the additional Mullite 15% by weight into 3Y-TZP system proved an increase of fracture toughness value up to 138% than pure 3Y-TZP system[/vc_column_text][vc_empty_space][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][vc_empty_space][megatron_heading title=”Author keywords” size=”size-sm” text_align=”text-left”][vc_column_text][/vc_column_text][vc_empty_space][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][vc_empty_space][megatron_heading title=”Indexed keywords” size=”size-sm” text_align=”text-left”][vc_column_text]Brittleness,Crack,Magnesia,Mullite,Y-TZP[/vc_column_text][vc_empty_space][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][vc_empty_space][megatron_heading title=”Funding details” size=”size-sm” text_align=”text-left”][vc_column_text][/vc_column_text][vc_empty_space][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][vc_empty_space][megatron_heading title=”DOI” size=”size-sm” text_align=”text-left”][vc_column_text]https://doi.org/10.1063/1.4930730[/vc_column_text][/vc_column_inner][vc_column_inner width=”1/4″][vc_column_text]Widget Plumx[/vc_column_text][/vc_column_inner][/vc_row_inner][/vc_column][/vc_row][vc_row][vc_column][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][/vc_column][/vc_row]