Enter your keyword

2-s2.0-85072647482

[vc_empty_space][vc_empty_space]

Effect of Aluminum and Silicon Antioxidants Addition on Porosity, Cold Crushing Strength, Wear Resistance and Hydration Effect of Alumina Spinel Refractories

Fernando E.D.a, Korda A.A.a

a Department of Metallurgical Engineering, Faculty of Mining and Petroleum Engineering, Bandung Institute of Technology, Indonesia

[vc_row][vc_column][vc_row_inner][vc_column_inner][vc_separator css=”.vc_custom_1624529070653{padding-top: 30px !important;padding-bottom: 30px !important;}”][/vc_column_inner][/vc_row_inner][vc_row_inner layout=”boxed”][vc_column_inner width=”3/4″ css=”.vc_custom_1624695412187{border-right-width: 1px !important;border-right-color: #dddddd !important;border-right-style: solid !important;border-radius: 1px !important;}”][vc_empty_space][megatron_heading title=”Abstract” size=”size-sm” text_align=”text-left”][vc_column_text]© 2019 Published under licence by IOP Publishing Ltd.Due to their high resistance and wear resistance, alumina spinel (MgAl2O4) are widely used for slide gate on ladle. The characteristics strongly depend on the formation of ceramic phases in the matrix. Addition of antioxidants is used to prevent the graphite oxidation, possibly leading to porosity increase. Currently, other problem appears as the consequences of climate change. The object of this research is to study the effect of antioxidants addition in temperature variations. The influence of Al and Si addition is investigated by means of XRD, SEM, TGA-DTA, apparent porosity, CCS, wear resistance and hydration resistance tests. It was found that lowest porosity, highest CCS and best wear resistance were reached by sample containing Al 5% in 1400°C, while best hydration resistance was reached by sample containing Si 5%.[/vc_column_text][vc_empty_space][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][vc_empty_space][megatron_heading title=”Author keywords” size=”size-sm” text_align=”text-left”][vc_column_text]Apparent porosity,Ceramic phasis,Cold crushing strengths,High resistance,Hydration effects,Hydration resistance,spinel,Temperature variation[/vc_column_text][vc_empty_space][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][vc_empty_space][megatron_heading title=”Indexed keywords” size=”size-sm” text_align=”text-left”][vc_column_text]antioxidant,CCS,hydration,porosity,spinel,wear resistance[/vc_column_text][vc_empty_space][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][vc_empty_space][megatron_heading title=”Funding details” size=”size-sm” text_align=”text-left”][vc_column_text][/vc_column_text][vc_empty_space][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][vc_empty_space][megatron_heading title=”DOI” size=”size-sm” text_align=”text-left”][vc_column_text]https://doi.org/10.1088/1757-899X/547/1/012008[/vc_column_text][/vc_column_inner][vc_column_inner width=”1/4″][vc_column_text]Widget Plumx[/vc_column_text][/vc_column_inner][/vc_row_inner][/vc_column][/vc_row][vc_row][vc_column][vc_separator css=”.vc_custom_1624528584150{padding-top: 25px !important;padding-bottom: 25px !important;}”][/vc_column][/vc_row]